Guide

BS 5534 and BS 8612: the ridge and verge fixing rules

Two British Standards govern how ridge, hip and verge pieces are held on. This guide sets out what each covers, what changed in 2014, and what a compliant mortar ridge and a compliant dry-fix ridge look like once built.

Ridge tiles sit at the highest and windiest point of a roof, and for a very long time they were held by one thing: a bed of mortar. Standards have moved on. BS 5534 is the British Standard that governs how slate and tile coverings are laid and fixed, and its 2014 revision changed how ridge, hip and verge parts are expected to be fixed. A second document, BS 8612, is what dry-fix products are tested against.

Neither document is a law that a homeowner has to read. Both shape what a competent roofer fits, what a manufacturer can say about a product and what a good quote should include. This guide explains them in plain terms, and keeps to what the manufacturer sources say about them. We do not have the standards' own text in front of us, so we do not quote clause numbers. For a quick yes or no on mortar, our short answer on mortar bedding settles it, and the ridge and verge service page lists the jobs these rules apply to.

What BS 5534 is, and why a ridge falls under it

BS 5534 deals with pitched roofs covered in slate or tile. It reaches past the covering itself to the timber battens, the underlay beneath and the way everything is fixed. The edition most often cited in manufacturers' literature is BS 5534:2014 with its later amendment, and Cupa Pizarras, the slate supplier, refers to it as BS 5534:2014+A2:2018.

To fix the terms: the ridge is the horizontal apex, a hip slopes down an external angle, and a verge finishes a slope against a gable. All three are finished with special pieces: ridge and hip tiles, and verge units or bedded edge tiles. Because they stand proud of the main covering, they take the full force of any wind that crosses the roof, and the standard treats them as parts of the covering that need their own fixings.

Why the top of a roof gets its own rules

The main field of a tiled roof is held down by its weight, its lap and its nails or clips. A ridge piece sits on a bed with only its own weight and the adhesion of mortar keeping it there. When wind rises over the roof it lifts those pieces first. That is why a ridge tile is so often the one found on the lawn after a gale, and it is the reasoning behind the fixing rules that follow. It also explains why the survey photographs the apex closely: one loose tile at the top can mean the bed beneath is failing along the whole run, and the quote has to reflect that.

What the 2014 revision changed

Marley's guidance, first published in 2016 and updated in February 2026, reads the 2014 revision as a turning point. Mortar's tensile strength, taken alone, stopped being something a roofer could trust with the job of holding ridge and hip pieces, and every bedded tile or fitting is now expected to be mechanically fixed too.

Read carefully, that is a narrower change than it is sometimes made to sound. It does not say mortar is banned. Nor does it say every mortar ridge laid before 2014 is defective. What it does say is that a bed of mortar can no longer be the sole means of holding a ridge or hip tile, so a bedded ridge carries a mechanical fixing too. The old assumption that a good bed was enough has gone.

What that means in the work

  • New ridges. A mortar-bedded ridge is built with mechanical fixings in addition to the bed.
  • Repairs and re-bedding. When tiles are lifted and bedded again, the fixings go in as part of the job, not as an optional extra.
  • Dry-fix. A mechanically fixed system with no bed at all is another way to meet the expectation, provided it is a tested one.

Our guide to ridge re-bedding follows a mortar re-bed through from strip to finish, and shows where the fixings come in. The same principle applies to verges and hips.

What BS 8612 tests

BS 8612 is the yardstick for dry-fixed ridge, hip and verge systems. Marley's position is that a dry product has to have passed proper testing before it can count towards compliance. The standard therefore gives manufacturers a shared way to prove their system, and gives roofers and homeowners a way to tell a proven system from one that merely looks like it.

On a data sheet, the claim the manufacturer makes for the whole system is what to hold the product to.

What testing is for

A dry system is a set of components: a batten or support, a union, clips and fixings, and the ridge or verge pieces themselves. The point of a test specification is that the parts are tested together, as a system, with the tile they are designed for. A union from one range and clips from another do not make a tested system just because each component has a data sheet.

What to look for in a product

  • A statement that the system is tested to BS 8612.
  • The tile profiles it was tested with.
  • The fixing type and number the test used.
  • Any limits on use, such as pitch or exposure.

Where the data sheet asks for a particular screw, we use that screw. Mixing fixings from one product with another is the quickest way to undo the point of the test. For the mechanics of a dry ridge, see our guide to dry ridge systems.

How a compliant mortar ridge is built

A mortar ridge built to current practice looks much like a traditional one from the ground, and the difference is in the fixings. The steps below describe the principle. The exact fixings and spacing come from the product or the specification for the job, so we follow those and do not offer a number of our own.

  1. Strip back. Old ridge tiles and failed mortar are cleared away, leaving bare the uppermost row and the timber beneath. Any rotten wood is cut out.
  2. Check the top courses. The row of tiles nearest the apex on each side is inspected for cracks and slipped laps, and swapped where it is not sound.
  3. Bed the tiles. Ridge tiles are laid on a mortar bed that fills the underside of the tile and forms a seal along each slope.
  4. Add the mechanical fixing. Each tile is tied back to the roof structure by a fixing that works without the mortar, normally a stainless-steel arrangement running to the ridge timber or a bracket.
  5. Point and finish. Joints and ends are pointed, and the mortar is struck off cleanly.

Mortar still earns its place here. It seals the joints against rain and gives each tile a level seat, which a fixing alone does not. The mechanical fixing means the tile stays in place if the mortar later cracks.

Hips and verges in mortar

A hip follows the same logic, with a further point at the foot: the lowest hip tile needs support against slipping, traditionally given by a hip iron. A mortar verge needs its edge tiles fixed as well as bedded. Our guide to hip tile repairs covers the hip detail.

How a compliant dry-fix ridge and verge are built

A dry system does without the mortar bed. It uses a timber batten fixed along the apex, a union strip closing the gap, clips that seat each tile and screws that hold the lot to the batten. A dry verge uses a continuous or unit section locked to the tile and the batten. Both exist in versions tested to BS 8612.

The early stages match a mortar job: the old ridge comes off and the uppermost rows of tiles are checked and mended if unsound. After that, the batten goes on, the union is laid, and the tiles are clipped and screwed down. Nothing depends on a cement bed setting, which means weather is less of a constraint on the day. Mortar work needs dry conditions and curing time; a dry ridge has no bed to wait on.

Where a dry system leaves less to chance

  • The fixings are visible and countable, so a survey photograph shows whether every tile is held.
  • There is no mortar to crack, shrink or wash out.
  • The components are specified, so a replacement tile can be fitted without disturbing the rest.

Where mortar remains the better fit

On a heritage roof, a traditional stone ridge or a conservation-area house, the look of a mortar joint can matter more than speed, and ask the council's planning team before choosing. A dry system also has to suit the tile. On an irregular old ridge line it may need packing out. Both methods can meet the standard if they are done properly, and the choice between them is discussed in our guide to mortar or dry-fix.

Checking a quote against the standards

Checking a ridge quote does not require the clauses. A few plain questions will do. Put them to any roofer, us included, before agreeing a price.

  • For a mortar ridge: does the quote say the tiles will have mechanical fixings in addition to the bed? If it speaks only of mortar, ask.
  • For a dry system: is the product named, with its BS 8612 test stated?
  • For a verge: are the edge tiles fixed mechanically, and is the undercloak (the strip beneath the edge tiles) checked?
  • For any ridge: does it mention the top course of tiles and the ridge timber?

Standards are not a guarantee on their own. A tested system fitted with the wrong screws, or a mortar ridge with fixings that miss the timber, will still fail. The workmanship decides the result.

What we do

We photograph the ridge, hips and verges from the roof at the survey and send you the pictures with the written quote. The quote covers access, removal of the old pieces, materials, fixings, labour and waste. We follow the manufacturer's data sheet for the fixings and spacing on your roof, and tell you which method we have specified and why.

Roofing work is normally charged with VAT, and your quote will show it. Our 10-year workmanship guarantee is on paper, and the site is left tidy. If you would like a ridge looked at, phone 01453 933613, send photographs on WhatsApp, or fill in the form on this site.

BS 5534 and BS 8612: specific questions

Does BS 5534:2014 make every older mortar ridge non-compliant?

Not as a ruling on a roof already built. The 2014 revision changed what is expected of new and repaired work: bedded ridge and hip tiles should include mechanical fixings. An older ridge is judged on its condition, and a survey shows whether it is sound or needs re-bedding.

Is a dry ridge automatically compliant because it has no mortar?

No. Only dry verge, ridge and hip products properly tested to BS 8612 count, and they need fitting to the manufacturer's instructions with the specified fixings. A kit without a test behind it does not gain compliance by being dry.

Who checks that a ridge was fixed to the standard?

For a ridge repair the evidence is the quote, the product data sheet and the photographs of the finished work. If the ridge is part of a larger re-roof, ask your building control body if the job is notifiable and which records it wants.

Get your roof priced

Tell us what's happening and we'll call you back with a time to look at it.

  • Guide prices before we visit
  • A written quote
  • 10-year workmanship guarantee

Rather talk? 01453 933613

Call Get a quote